Gate Blush Halo or Blush Marks Circular pattern around gate, Generally only an issue on very hot runner molds Injection velocity is simply too fast, gate/sprue/runner dimensions is simply too smaller, or perhaps the melt/mildew temp is too low. We've figured out from encounter that, in advance of manufacturing begins, https://thesocialintro.com/story3617509/the-smart-trick-of-plastic-injection-molding-manufacturer-that-nobody-is-discussing